Stress Corrosion Cracking of X-70 steel in carbonates, solutions

Stress Corrosion Cracking of X-70 Microalloyed steel in carbonates, chlorides and sulfates solutions

LAP LAMBERT Academic Publishing (18.10.2011 )

Books loader

Omni badge gutscheinfähig
ISBN-13:

978-3-8465-3471-7

ISBN-10:
3846534714
EAN:
9783846534717
Buchsprache:
Englisch
Klappentext:
The aim of this work was to study the effect of different heat treatments on the stress corrosion cracking (SCC) resistance of X-70 pipeline steel in diluted solutions of NaHCO3 (0.1 M, 0.05 M, 0.01 M, and 0.005 M), and in solutions of NaHCO3 with addition of KCl, CaCl2 and MgSO4-7H2O, using the slow strain rate testing (SSRT) technique,and some heat treatments.The results obtained indicated that the quenched and quenched+tempered conditions are the only ones susceptible to HE and the mechanism of SCC in X-70 pipeline steel increased in most diluted solution of NaHCO3 at 50C, and was dominated by film rupture an anodic dissolution.
Verlag:
LAP LAMBERT Academic Publishing
Webseite:
https://www.lap-publishing.com/
von (Autor):
Alvaro Torres, Sergio Serna, Bernardo Campillo
Seitenanzahl:
60
Veröffentlicht am:
18.10.2011
Lagerbestand:
Lieferbar
Kategorie:
Chemische Technik
Preis:
49,00 €
Stichworte:
SCC Electrochemical, Microalloyed Steel

Books loader

Newsletter

Adyen::amex Adyen::mc Adyen::visa Adyen::cup Adyen::unionpay Paypal CryptoWallet Überweisung

  0 Produkte im Warenkorb
Warenkorb bearbeiten
Loading frontend
LOADING